Mechanical Properties Metric English Comments
Shear Modulus 1.10 GPa
160 ksi
Calculated
Network Polymers Kepital® F20-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Shear Modulus 1.10 GPa
160 ksi
calculated
BASF Capron® 8202 NL Nylon 6 (Dry)  (discontinued **)
Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta..
Shear Modulus 1.10 GPa
160 ksi
Calculated
Hexcel® HexPly® F593 Epoxy Resin
HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo..