Polymer Property : Shear Modulus = 1.18 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.00817 GPa
1.18 ksi
Calculated
Arlon CP-594CX Bulk Compound
Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but ..