Arlon CP-594CX Bulk Compound

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon CP-594CX Bulk Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but is not recognized by Underwriters Laboratories.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
Silicone Property; Arlon SQA-TMS-024
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Silicone Property; ASTM D2240
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 24.5 MPa

@Strain <=1.00 %
3550 psi

@Strain <=1.00 %
Silicone Property; Arlon-SAQ-TMS-008
Elongation at Break 125 %
125 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.00817 GPa
1.18 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 111 µm/m-°C

@Temperature 20.0 - 160 °C
61.7 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.820 J/g-°C

@Temperature 100 °C
0.196 BTU/lb-°F

@Temperature 212 °F
Silicone Property; E1461-01
Thermal Conductivity 1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg -118 °C
-180 °F
Silicone Property; ASTM D3418
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 6.9

@Frequency 1.00e+6 Hz
6.9

@Frequency 1.00e+6 Hz
D<sub>k</sub>, Silicone Property; IPC TM 650-2.5.5.3
Dissipation Factor 0.0044

@Frequency 1.00e+6 Hz
0.0044

@Frequency 1.00e+6 Hz
D<sub>f</sub>, Silicone Property; IPC TM 650-2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.101 - 0.345 MPa,
Temperature 121.0 °C
0.250 hour

@Pressure 14.6 - 50.0 psi,
Temperature 249.8 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 7.00 °C
6.00 Month

@Temperature 44.6 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Plasticity 2.3 mm
Arlon SQA-TMS-005