Mechanical Properties Metric English Comments
Shear Modulus 1.65 - 4.22 GPa
239 - 611 ksi
Average value: 2.51 GPa Grade Count:3
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..