Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.96 - 2.68 GPa | 285 - 388 ksi | Average value: 2.37 GPa Grade Count:3 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |