Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 8.80 GPa | 1280 ksi | Calculated |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |