Polymer Property : Shear Modulus = 8.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 8.80 GPa
1280 ksi
Calculated
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..