Polymer Property : Shear Modulus = 194 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.34 GPa
194 ksi
ISO R527 type 1
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix
HexPly® 924 is a controlled flow epoxy matrix developed for the fabrication of high temperature resistant primary structures. When cured, HexPly® 924 becomes a tough composite with high impact res..