Polymer Property : Shear Modulus = 232 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.60 - 4.40 GPa
232 - 638 ksi
Average value: 3.15 GPa Grade Count:8
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Shear Modulus 1.60 GPa
232 ksi
calculated
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength..