Shear Modulus 1.60 - 4.40 GPa
232 - 638 ksi
Average value: 3.15 GPa Grade Count:8
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..