Mechanical Properties Metric English Comments
Shear Modulus 3.60 GPa
522 ksi
calculated
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc..
Shear Modulus 3.60 GPa
522 ksi
calculated
BASF Capron® GR630 30% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron GR630 is a 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineering..
Shear Modulus 3.60 GPa
522 ksi
calculated
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Shear Modulus 3.60 GPa
522 ksi
calculated
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba..