Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.60 GPa | 522 ksi | calculated |
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Shear Modulus | 3.60 GPa | 522 ksi | calculated |
BASF Capron® GR630 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 is a 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineering.. |
|||
Shear Modulus | 3.60 GPa | 522 ksi | calculated |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Shear Modulus | 3.60 GPa | 522 ksi | calculated |
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba.. |