Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.92 - 4.25 GPa | 569 - 616 ksi | Calculated |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |