Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.33 - 4.65 GPa | 628 - 674 ksi | Calculated |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |