Mechanical Properties Metric English Comments
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC
Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP
SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP
SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product ..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP
SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP
SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are ..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP
SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP
SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in ..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP
SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP
SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e..
Shear Modulus 4.20 GPa
609 ksi
in plane
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP
SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific..
Shear Modulus 4.20 GPa
609 ksi
Calculated
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..