Mechanical Properties Metric English Comments
Shear Modulus 5.98 GPa
867 ksi
Calculated
Plenco 6401 Phenolic, Briquette, Injection Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.