Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.20 g/micron @Temperature 23.0 °C |
81.3 g/mil @Temperature 73.4 °F |
ASTM 1709A |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Dart Drop | 3.20 g/micron @Temperature -18.0 °C |
81.3 g/mil @Temperature -0.400 °F |
ASTM 1709A |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Dart Drop | 3.20 g/micron @Temperature -30.0 °C |
81.3 g/mil @Temperature -22.0 °F |
ASTM 1709A |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |