Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 13.1 MPa | 1900 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1327CA Blown Film Resin
(discontinued **) Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, TD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Film Tensile Strength at Yield, TD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
Film Tensile Strength at Yield, TD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Film Tensile Strength at Yield, TD | 13.1 MPa | 1900 psi | at 2% offset; ASTM D882 |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Film Tensile Strength at Yield, TD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil HD 7845.30 MMW Blown Film Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |