ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name Nexxstar™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.Availability: Latin America, North America and South AmericaAdditive: Antiblock: NoSlip: No Thermal Stabilizer: NoInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
Melt Flow 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.1 MPa
1900 psi
ASTM D882
Film Elongation at Break, MD 450 %
450 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Elmendorf Tear Strength MD 200 g
200 g
ASTM D1922
Elmendorf Tear Strength TD 300 g
300 g
ASTM D1922
Dart Drop Test 130 g
0.287 lb
ASTM D1709A
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Film Tensile Strength at Break, TD 28.3 MPa
4100 psi
ASTM D882
1% Secant Modulus, MD 262 MPa
38000 psi
ASTM D882
1% Secant Modulus, TD 283 MPa
41000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 239 °C
<= 462 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 68 %
68 %
45°; ASTM D2457