Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 9.58 MPa | 1390 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 9.58 MPa | 1390 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 9.60 MPa | 1390 psi | ASTM D882-02 |
Ipiranga Petrochem LTH 0212 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |