Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 14.8 MPa | 2150 psi | ASTM D882 |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Film Tensile Strength at Yield, TD | 14.8 MPa | 2140 psi | ASTM D882 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |