Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 100 - 160 MPa
14500 - 23200 psi
Average value: 130 MPa Grade Count:17
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..