Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, TD = 14500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 1311 Polyester Film
Melinex® 1311 is a clear polyester film with antistatic properties on both surfaces for improved web handling and safety.Information provided by DuPont.
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 197 Polyester Film
Melinex® 197 is a very clear polyester film with good handling properties, suitable for general purpose applications.Information provided by DuPont.
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 313 Polyester Film
Melinex® 313 is a general purpose polyester film with consistently good handling properties. It is pretreated on one side for adhesion.Information provided by DuPont.
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 515 Polyester Film
A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Typical Applications: MELINEX® 515 is suitable for applications which ..
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 582 Polyester Film, 400 Gauge
Melinex® 582 is a high clarity polyester film which is two-side hydrophilic pretreated to promote adhesion to many industrial aqueous coating and inks.Approvals: UL Recognition - Product has been r..
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge
Melinex® FRPS is a lower shrinkage version of Melinex® S. Designed specifically for release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and ..
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 516 Polyester Film
Melinex® 516 is a high clarity polyester film which is pretreated on both sides for slip to combine good handling properties with high clarity and brilliance.Typical Applications: Some typical uses..
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 516D Polyester Film
A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Information provided by DuPont.
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882
CEN® Electronic Material HT Polyimide Film
CEN® HT is a one side or both sides electrically conductive polyimide film for heating applications. With precisely controlled surface resistivity, the film resistive property is retained througho..
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
DuPont Teijin Films Melinex® 516R Polyester Film
A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brillianceInformation provided by DuPont.
Film Tensile Strength at Yield, TD 100 - 160 MPa
14500 - 23200 psi
Average value: 130 MPa Grade Count:17
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..