Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 27.0 MPa
3920 psi
ASTM D882
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin
Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Film Tensile Strength at Yield, TD 27.0 MPa
3920 psi
ASTM D882
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..