Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ISO 527-3 |
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:.. |
|||
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured.. |
|||
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ISO 527-3 |
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,.. |
|||
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ISO 527-3 |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ASTM D882 |
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ISO 527-3 |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Film Tensile Strength at Yield, TD | 5.00 MPa | 725 psi | ISO 527-3 |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Film Tensile Strength at Yield, TD | 5.00 - 66.9 MPa | 725 - 9700 psi | Average value: 12.0 MPa Grade Count:11 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Film Tensile Strength at Yield, TD | 5.00 - 46.0 MPa | 725 - 6670 psi | Average value: 10.9 MPa Grade Count:120 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |