Polymer Property : Film Tensile Strength at Yield, TD = 5370 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 37.0 MPa
5370 psi
ASTM D882
Reliance Industries Relene F56003 Polyethylene
Relene F56003 is a High Density Polyethylene grade suitable for producing blown parts with excellent drawdown and paper like feel. It is recommended for making carrier bags and coextruded film stru..