Polymer Property : Elmendorf Tear Strength, MD = 0.512 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD >= 0.512 g/micron
>= 13.0 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD >= 0.512 g/micron
>= 13.0 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 0.512 g/micron
13.0 g/mil
ASTM D1922
Formosa Plastics Formolene® E905 Film HDPE  (discontinued **)
HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve..
Elmendorf Tear Strength, MD 0.512 g/micron
13.0 g/mil
Notched; ASTM D1922
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin
Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not..