Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.748 g/micron | 19.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Elmendorf Tear Strength, MD | 0.748 g/micron | 19.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Elmendorf Tear Strength, MD | 0.748 g/micron | 19.0 g/mil | Calculated from mfr's report of 1.9 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |