Polymer Property : Elmendorf Tear Strength, MD = 0.8152 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.8152 g/micron
20.71 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene
Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug..
Elmendorf Tear Strength, MD 0.8152 g/micron
20.71 g/mil
ISO 6383-2
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene
Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco..