Polymer Property : Elmendorf Tear Strength, MD = 1.50 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.50 g/micron
38.1 g/mil
ISO 6383-2
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T..
Elmendorf Tear Strength, MD 1.50 g/micron
38.1 g/mil
ISO 6383-2
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film
Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P..
Elmendorf Tear Strength, MD 1.50 g/micron
38.1 g/mil
ASTM D1922
Eastman Tritan FX200 Copolyester
Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..