Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 14.3 g/micron | 364 g/mil | Cast Film at 2.0 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 2121 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: Good processabilityGood drawdownEdge tear resistanceLow neck-in Applications: Typical cast film applicatio.. |