Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 14.3 g/micron
364 g/mil
Cast Film at 2.0 mil; ASTM D-1922
Chevron Phillips MarFlex® 2121 Polyethylene; LDPE
Low density polyethylene. This LDPE is tailored for cast film applications that require: Good processabilityGood drawdownEdge tear resistanceLow neck-in Applications: Typical cast film applicatio..