Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.4374 - 0.6016 g/micron
11.11 - 15.28 g/mil
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..