Material Notes:
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock. 1530 is a PVDC-Coated product, providing improved moisture and oxygen barrier while retaining superior clarity.Applications: bag-on-box packaging, packaging for processed meats, cheese, meat snacks, coffee bricks, coffee bags, and pet food, agricultural bags, stand-up shampoo pouches, book covers and metallized balloons.Information provided by Honeywell.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0450 lb/in³
Yield Density
Water Vapor Transmission 9.31 - 12.42 g/m²/day
0.600 - 0.7998 g/100 in²/day
100°F / 100%RH); ASTM F1249
Oxygen Transmission Rate 9.31 - 13.97 cc/m²/day
0.600 - 0.8997 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Thickness 18.3 microns
0.720 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 60 - 110 %
60 - 110 %
ASTM D882
Film Elongation at Break, TD 60 - 110 %
60 - 110 %
ASTM D882
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Coefficient of Friction 0.18 - 0.27
0.18 - 0.27
film to stainless steel; ASTM D1894
0.59 - 0.90
0.59 - 0.90
film to film; ASTM D1894
Tear Strength Test 1100 - 1500
1100 - 1500
graves tear, grams/mil (initial); ASTM D1004
Elmendorf Tear Strength, MD 0.4374 - 0.6016 g/micron
11.11 - 15.28 g/mil
Film Tensile Strength at Break, MD 221 - 303 MPa
32000 - 44000 psi
ASTM D882
Film Tensile Strength at Break, TD 200 - 283 MPa
29000 - 41000 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD 1.4 - 2.4 %
1.4 - 2.4 %
320°F / 160°C - 5 minutes; ASTM D1204
Shrinkage, TD 0.20 - 0.70 %
0.20 - 0.70 %
320°F / 160°C - 5 minutes; ASTM D1204
Optical Properties Metric English Comments
Haze <= 5.0 %
<= 5.0 %
ASTM D1003
Gloss 75 - 85 %
75 - 85 %
at 20°