Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 2.64 g/micron
67.0 g/mil
ASTM D1922
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all..
Elmendorf Tear Strength, MD 2.64 g/micron
67.0 g/mil
Calculated from mfr's report of 3.4 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..