Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.18 g/micron
30.0 g/mil
Notched; ASTM D1922
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin  (discontinued **)
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In..
Elmendorf Tear Strength, MD 1.18 - 3.15 g/micron
30.0 - 80.0 g/mil
Honeywell Capran® Unidraw (1.00 mil) Nylon 6 Film  (discontinued **)
Description: Capran® Unidraw is a 1.00 mil (25 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str..
Elmendorf Tear Strength, MD 1.18 g/micron
30.0 g/mil
4 BUR; ASTM D1922
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film
This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica..
Elmendorf Tear Strength, MD 1.18 g/micron
30.0 g/mil
ASTM D882
Dow DAF 780 Carpet Underlayment Adhesion Film
DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow