Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 12.3 g/micron | 312 g/mil | |
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev.. |