Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
ASTM D1922
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin
Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
ASTM D1922
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile..
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
ASTM D1922
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre..
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
ASTM D1922
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
ASTM D1922
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
ASTM D1922
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin
Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac..
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. ..
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1..
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade
DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an..