Material Notes:
DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
Thickness 40.0 microns
1.57 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg
2.0 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.4 MPa
1650 psi
Film Tensile Strength at Yield, TD 10.3 MPa
1490 psi
Film Elongation at Break, MD 290 %
290 %
Film Elongation at Break, TD 560 %
560 %
Coefficient of Friction 0.10
0.10
Elmendorf Tear Strength MD 520 g
520 g
Elmendorf Tear Strength TD 250 g
250 g
Elmendorf Tear Strength, MD 13.0 g/micron
330 g/mil
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
Dart Drop 2.40 g/micron
61.0 g/mil
Film Tensile Strength at Break, MD 25.9 MPa
3760 psi
Film Tensile Strength at Break, TD 17.6 MPa
2550 psi
Optical Properties Metric English Comments
Haze 8.5 %
8.5 %
Gloss 61 %
61 %
45°
Processing Properties Metric English Comments
Processing Temperature 191 °C
376 °F
Film extrusion temperature