Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured.. |
|||
Elmendorf Tear Strength, MD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi.. |
|||
Elmendorf Tear Strength, MD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability.. |