Elmendorf Tear Strength, MD 17.3 g/micron
440 g/mil
ASTM D1922
Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: processing aid additiveCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPEApplications: thick or t..
Elmendorf Tear Strength, MD 17.3 g/micron
440 g/mil
ASTM D1922
Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Elmendorf Tear Strength, MD 17.3 g/micron
440 g/mil
ASTM D1922
ExxonMobil LL 3301.34 Premium High Strength Film Resin  (discontinued **)
LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi..
Elmendorf Tear Strength, MD 17.3 g/micron
440 g/mil
ASTM D1922
ExxonMobil LL 3301.63 Premium High Strength Film Resin  (discontinued **)
LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi..