Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.65 g/micron | 194 g/mil | ISO 6383/2 |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Elmendorf Tear Strength, MD | 7.65 g/micron | 194 g/mil | ISO 6383/2 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Elmendorf Tear Strength, MD | 7.65 g/micron | 194 g/mil | ISO 6383/2 |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |