Polymer Property : Elmendorf Tear Strength, TD = 0.945 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 0.945 - 9.06 g/micron
24.0 - 230 g/mil
Average value: 3.59 g/micron Grade Count:68
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Elmendorf Tear Strength, TD 0.945 g/micron
24.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile..