Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 10.19 g/micron
258.8 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene
Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug..
Elmendorf Tear Strength, TD 10.19 g/micron
258.8 g/mil
ISO 6383-2
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene
Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C..