Polymer Property : Elmendorf Tear Strength, TD = 124 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 4.89 g/micron
124 g/mil
ISO 6383/2
Borealis FA3220 Low Density Polyethylene
FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has bee..
Elmendorf Tear Strength, TD 4.89 g/micron
124 g/mil
ISO 6383/2
Borealis FA3227 Low Density Polyethylene
FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al..
Elmendorf Tear Strength, TD 4.90 g/micron
124 g/mil
ASTM-D1922
Braskem TN2020 EVA General Film Copolymer
TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures..