Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.89 g/micron | 124 g/mil | ISO 6383/2 |
Borealis FA3220 Low Density Polyethylene FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has bee.. |
|||
Elmendorf Tear Strength, TD | 4.89 g/micron | 124 g/mil | ISO 6383/2 |
Borealis FA3227 Low Density Polyethylene FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al.. |