Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 13.68 g/micron | 347.5 g/mil | ASTM-D1922 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |