Elmendorf Tear Strength, TD 13.68 g/micron
347.5 g/mil
ASTM-D1922
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan..