Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 5.35 g/micron | 136 g/mil | ASTM D1922 |
Eastman 184MF Polyethylene Film
(discontinued **) Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character.. |
|||
Elmendorf Tear Strength, TD | 5.35 g/micron | 136 g/mil | ASTM D1922 |
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve.. |