Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 0.551 g/micron
14.0 g/mil
ASTM D1922
NatureWorks® Ingeo™ 4032D Film Grade PLA
NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce..